Kinetics of the Glass Transition of Silica-Filled Styrene–Butadiene Rubber: The Effect of Resins

Zur Kurzanzeige

dc.identifier.uri http://dx.doi.org/10.15488/12733
dc.identifier.uri https://www.repo.uni-hannover.de/handle/123456789/12833
dc.contributor.author Lindemann, Niclas
dc.contributor.author Schawe, Jürgen E. K.
dc.contributor.author Lacayo-Pineda, Jorge
dc.date.accessioned 2022-09-08T07:59:16Z
dc.date.available 2022-09-08T07:59:16Z
dc.date.issued 2022
dc.identifier.citation Lindemann, N.; Schawe, J.E.K.; Lacayo-Pineda, J.: Kinetics of the Glass Transition of Silica-Filled Styrene–Butadiene Rubber: The Effect of Resins. In: Polymers 14 (2022), Nr. 13, 2626. DOI: https://doi.org/10.3390/polym14132626
dc.description.abstract Resins are important for enhancing both the processability and performance of rubber. Their efficient utilization requires knowledge about their influence on the dynamic glass transition and their miscibility behavior in the specific rubber compound. The resins investigated, poly-(α-methylstyrene) (AMS) and indene-coumarone (IC), differ in molecular rigidity but have a similar aromaticity degree and glass transition temperature. Transmission electron microscopy (TEM) investigations show an accumulation of IC around the silanized silica in styrene–butadiene rubber (SBR) at high contents, while AMS does not show this effect. This higher affinity between IC and the silica surface leads to an increased compactness of the filler network, as determined by dynamic mechanical analysis (DMA). The influence of the resin content on the glass transition of the rubber compounds is evaluated in the sense of the Gordon–Taylor equation and suggests a rigid amorphous fraction for the accumulated IC. Broadband dielectric spectroscopy (BDS) and fast differential scanning calorimetry (FDSC) are applied for the characterization of the dielectric and thermal relaxations as well as for the corresponding vitrification kinetics. The cooling rate dependence of the vitrification process is combined with the thermal and dielectric relaxation time by one single Vogel–Fulcher–Tammann–Hesse equation, showing an increased fragility of the rubber containing AMS. eng
dc.language.iso eng
dc.publisher Basel : MDPI
dc.relation.ispartofseries Polymers 14 (2022), Nr. 13
dc.rights CC BY 4.0 Unported
dc.rights.uri https://creativecommons.org/licenses/by/4.0/
dc.subject glass transition eng
dc.subject kinetics eng
dc.subject rubber eng
dc.subject resin eng
dc.subject BDS eng
dc.subject FDSC eng
dc.subject.ddc 540 | Chemie ger
dc.title Kinetics of the Glass Transition of Silica-Filled Styrene–Butadiene Rubber: The Effect of Resins
dc.type Article
dc.type Text
dc.relation.essn 2073-4360
dc.relation.doi https://doi.org/10.3390/polym14132626
dc.bibliographicCitation.issue 13
dc.bibliographicCitation.volume 14
dc.bibliographicCitation.firstPage 2626
dc.description.version publishedVersion
tib.accessRights frei zug�nglich


Die Publikation erscheint in Sammlung(en):

Zur Kurzanzeige

 

Suche im Repositorium


Durchblättern

Mein Nutzer/innenkonto

Nutzungsstatistiken