Reliable copper spot welding with ir laser radiation through short prepulsing

Zur Kurzanzeige

dc.identifier.uri http://dx.doi.org/10.15488/4646
dc.identifier.uri https://www.repo.uni-hannover.de/handle/123456789/4688
dc.contributor.author Moalem, A.
dc.contributor.author Von Witzendorff, Philipp
dc.contributor.author Stute, U.
dc.contributor.author Overmeyer, Ludger
dc.date.accessioned 2019-03-28T10:21:33Z
dc.date.available 2019-03-28T10:21:33Z
dc.date.issued 2012
dc.identifier.citation Moalem, A.; Von Witzendorff, P.; Stute, U.; Overmeyer, L.: Reliable copper spot welding with ir laser radiation through short prepulsing. In: Procedia CIRP 3 (2012), Nr. 1, S. 459-464. DOI: https://doi.org/10.1016/j.procir.2012.07.079
dc.description.abstract We demonstrate a technique, which significantly enhances the stability of copper welding with laser radiation. After modelling spot welding stability we conclude that oxide layer morphology typical for native oxide layers has to be avoided. We locally normalize the surface oxidation degree using laser pulses in the nanosecond pulse duration regime (short prepulsing). Thereby, the absorptivity is reliably increased, setting uniform starting conditions for laser welding. A process window is identified, where all experimental repetitions lead to successful welds. With prepulsing, the spot weld diameter variation is decreased to 2% and the necessary welding energy is decreased up to 40%. eng
dc.language.iso eng
dc.publisher Amsterdam : Elsevier B.V.
dc.relation.ispartofseries Procedia CIRP 3 (2012), Nr. 1
dc.rights CC BY-NC-ND 3.0 Unported
dc.rights.uri https://creativecommons.org/licenses/by-nc-nd/3.0/
dc.subject Copper eng
dc.subject Laser eng
dc.subject Prepulsing eng
dc.subject Reliability eng
dc.subject Stability eng
dc.subject Welding eng
dc.subject Convergence of numerical methods eng
dc.subject Copper eng
dc.subject Laser beam welding eng
dc.subject Laser radiation eng
dc.subject Lasers eng
dc.subject Manufacture eng
dc.subject Reliability eng
dc.subject Welding eng
dc.subject Welds eng
dc.subject Absorptivities eng
dc.subject Diameter variation eng
dc.subject Nanosecond pulse eng
dc.subject Native oxide layer eng
dc.subject Prepulsing eng
dc.subject Surface oxidations eng
dc.subject Welding energy eng
dc.subject Welding stability eng
dc.subject Spot welding eng
dc.subject.classification Konferenzschrift ger
dc.subject.ddc 600 | Technik ger
dc.subject.ddc 670 | Industrielle und handwerkliche Fertigung ger
dc.title Reliable copper spot welding with ir laser radiation through short prepulsing
dc.type Article
dc.type Text
dc.relation.issn 2212-8271
dc.relation.doi https://doi.org/10.1016/j.procir.2012.07.079
dc.bibliographicCitation.issue 1
dc.bibliographicCitation.volume 3
dc.bibliographicCitation.firstPage 459
dc.bibliographicCitation.lastPage 464
dc.description.version publishedVersion
tib.accessRights frei zug�nglich


Die Publikation erscheint in Sammlung(en):

  • An-Institute
    Frei zugängliche Publikationen aus An-Instituten der Leibniz Universität Hannover

Zur Kurzanzeige

 

Suche im Repositorium


Durchblättern

Mein Nutzer/innenkonto

Nutzungsstatistiken