Classification of defective regions in p-type multicrystalline silicon by comparing luminescence images measured under different conditions

Show simple item record

dc.identifier.uri http://dx.doi.org/10.15488/4041
dc.identifier.uri https://www.repo.uni-hannover.de/handle/123456789/4075
dc.contributor.author Krain, Rafael
dc.contributor.author Beljakova, Svetlana
dc.contributor.author Herlufsen, Sandra
dc.contributor.author Krieger, Michael
dc.contributor.author Schmidt, Jan
dc.date.accessioned 2018-11-27T08:24:25Z
dc.date.available 2018-11-27T08:24:25Z
dc.date.issued 2013
dc.identifier.citation Krain, R.; Beljakova, S.; Herlufsen, S.; Krieger, M.; Schmidt, J.: Classification of defective regions in p-type multicrystalline silicon by comparing luminescence images measured under different conditions. In: Energy Procedia 38 (2013), S. 101-107. DOI: https://doi.org/10.1016/j.egypro.2013.07.255
dc.description.abstract In this contribution, we apply three different camera-based luminescence imaging techniques to mc-Si wafers and solar cells, fabricated on neighboring wafers. On wafer level, we determine the spatially-resolved carrier lifetime using calibrated photoluminescence lifetime imaging. On the solar cell level, we use band-to-band electroluminescence and sub-band-gap electroluminescence imaging for the characterisation. We analyze the differences obtained by the different techniques in specific defective areas. Characteristic regions are additionally examined using deep-level transient spectroscopy (DLTS). Comparing different luminescence images, we find different signal correlations in selected regions of the wafers and the neighboring cells presumably caused by different types of defects, which react more or less effective on the phosphorus gettering during the solar cell process. DLTS spectra show that in the edge region of the wafer close to the crucible, FeB pairs are present in the wafer as well as in the cell. However, the FeB concentration in the cell is, due to phosphorus gettering during the cell process, reduced by one order of magnitude. In regions which appear as very recombination-active defect clusters in the solar cell, we detect ZnB pairs by DLTS analysis. Note that the ZnB itself is a shallow centre and therefore expected to be not strong recombination active. However, our measurements reveal that Zn is present in regions with increased recombination activity, which is also in good agreement with the high total Zn concentration measured in the mc-Si ingot. We hence conjecture that dislocation clusters decorated by Zn are responsible for the non-getterable defect regions. eng
dc.language.iso eng
dc.publisher London : Elsevier Ltd.
dc.relation.ispartofseries Energy Procedia 38 (2013)
dc.rights CC BY-NC-ND 3.0 Unported
dc.rights.uri https://creativecommons.org/licenses/by-nc-nd/3.0/
dc.subject Defects eng
dc.subject luminescence eng
dc.subject multicrystalline silicon eng
dc.subject DLTS eng
dc.subject FeB eng
dc.subject ZnB eng
dc.subject.classification Konferenzschrift ger
dc.subject.ddc 620 | Ingenieurwissenschaften und Maschinenbau ger
dc.title Classification of defective regions in p-type multicrystalline silicon by comparing luminescence images measured under different conditions
dc.type Article
dc.type Text
dc.relation.issn 1876-6102
dc.relation.doi https://doi.org/10.1016/j.egypro.2013.07.255
dc.bibliographicCitation.volume 38
dc.bibliographicCitation.firstPage 101
dc.bibliographicCitation.lastPage 107
dc.description.version publishedVersion
tib.accessRights frei zug�nglich


Files in this item

This item appears in the following Collection(s):

  • An-Institute
    Frei zugängliche Publikationen aus An-Instituten der Leibniz Universität Hannover

Show simple item record

 